Sign In | Join Free | My wneducation.com
China Anhui Hechuang New Synthetic Materials Co., Ltd logo
Anhui Hechuang New Synthetic Materials Co., Ltd
Anhui Hechuang New Synthetic Materials Co., Ltd
Verified Supplier

3 Years

Home > HDPE Geomembrane Sheet >

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Anhui Hechuang New Synthetic Materials Co., Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

  • 1
  • 2

Brand Name : Geomax

Model Number : Geomembrane

Certification : CE

Place of Origin : ANHUI CHINA

MOQ : 1000 Square Meter

Price : Negotiation

Payment Terms : T/T, L/C

Supply Ability : 10000suqre Mater/Day

Delivery Time : 7 -20days

Packaging Details : Packed in The Woven Bags orCcustomized

Material : HDPE LDPE LLDPE PVC PE

Length : 50-200m

Width : 1m~8m

Thickness : 0.2mm~3mm

Transport Package : HDPE Geomembrane Liner Is Packed in The Woven Bags

Specification : 0.5mm 0.75mm 1.0mm 1.5mm 2mm

Origin : Anhui, China

Application : Transportation Project, Hydraulic Project, Geotechnical Project, Environmental Project

Contact Now

PRODUCT DESCRIPTION

Smooth Textured HDPE LDPE LLDPE PVC Geomembrane For Dam Pond Liner Landfill Mining

Product Introduction

Construction Method
1. The slope shall be laid in order from top to bottom. Don't pull it too tight.
2. Tow adjacent longitudinal joints should not be in a horizontal line, should bestaggered more than 1m each other.
3. Longitudinal joints should be more than 1.50m away from the dam foot and bending foot, and should be located on the plane.
4. When the slope is laid, the direction of spreading film should be basically parallel to the slope line.
5. The construction, first of all to use small diameter sand or clay levelingbase, and then laid the geomembrane. The geomembrane should not be stretched too tight, and the part of the soil bured at both ends is corrugated. A transitional layer of about 10cm is laid on the geomembrane with sand or clay.

Specifications

Specification Test method Unit Type
thickness ASTM 05199 mm 0.75 1 1.25 1.5 2
density ASTM 0 1505 g/cm3. min. 0.939 0.939 0.939 0.939 0.939
tensile strength at yield ASTM 06693 KN/m. min. 11 15 18 22 29
tensile strength at break ASTM 06693 KN/m. min. 20 27 33 40 53
elongation at yield ASTM 06693 %.max. 12 12 12 12 12
elongation at break ASTM 06693 %.max. 700 700 700 700 700
tear resistance ASTM 0 1004 N 93 125 156 187 249
puncture resistance ASTM 04833 N 240 320 400 480 640
environment stress cracking resistance ASTM 05397 hr 300 300 300 300 300
carbon black content ASTM 0 1603 % 2-3 2-3 2-3 2-3 2-3
oxidation induction time (OIT) ASTM 03895 minute 100 100 100 100 100
low temperature
(-70'C)impact brittle
ASTM 02136 pass pass pass pass pass
stream hydraulic conductivity g.cm/(cm².s.Pa),
max.
1x10¯13 1x10¯13 1x10¯13 1x10¯13 1x10¯13
dimension stability after 2 storge 1 h/100'C ASTM 0 1204 %.max 2 2 2 2 2

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining


HCNS Manufacture

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Exhibition 30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining

Our Certificates and HDPE Geocell Testing reports

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining


Product Tags:

LDPE hdpe geomembrana

      

30 mils hdpe geomembrana

      

Landfill geomembrana hdpe 30 mils

      
Buy cheap 30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining product

30 Mils LDPE LLDPE PVC HDPE Geomembrana For Dam Pond Liner Landfill Mining Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Anhui Hechuang New Synthetic Materials Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)